Abstract

LESCALLOY 35NCD16 Vac-Arc steel has superior cleanliness resulting in a combination of high strength and good fracture toughness. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on heat treating. Filing Code: SA-456. Producer or source: Latrobe Steel Company.