Abstract

CLR 95 TRANSPARENT GRADE is a MAGNUM ABS resin specifically designed for transparency. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. Filing Code: P-23. Producer or source: The Dow Chemical Company, Dow Plastics.