AlSiMag 870/871 is a 96% Al2O3 high quality alumina designed for electronic and mechanical applications This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive and bend strength as well as fracture toughness. Filing Code: Cer-8. Producer or source: AlSiMag Technical Ceramics Inc..