Abstract

VANADIS 4 is a high performance cold work tool steel made by powder metallurgy. It offers an extremely good combination of resistance and toughness for high performance tools. This datasheet provides information on composition, physical properties, hardness, elasticity, and bend strength as well as fracture toughness. It also includes information on heat treating and machining. Filing Code: TS-506. Producer or source: Uddeholm Corporation.