Refractory Sheet Type 100 is an engineered ceramic, fiber reinforced structural alumina composite with useful properties in thermal, structural and electrical insulation applications; as well as the transport of molten nonferrous metals to 1260 C (2300 F). This datasheet provides information on composition, physical properties, and compressive strength. It also includes information on corrosion resistance as well as machining. Filing Code: Cp-19. Producer or source: Zircar Products Inc..