Abstract

AA 6063 is a precipitation hardenable alloy; the hardening constituent being Mg2Si. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-320. Producer or source: Various aluminum companies.