Abstract

REZISTAL 310 is an austenitic chromium-nickel stainless steel with high heat resisting properties. It is particularly suited to intermittent heating and cooling. It is equivalent to AISI Type 310 stainless steel. Type 310S has lower carbon content, namely, 0.08 maximum. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-33. Producer or source: Crucible Steel Company of America.