Abstract

NILVAR is a 36% nickel-iron alloy having the lowest coefficient of expansion, recommended for applications requiring no dimensional changes with temperature variations. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Fe-8. Producer or source: Driver-Harris Company.