Abstract

Hiduminium RR.77 is a precipitation hardening aluminum alloy possessing specific strength properties equal to or exceeding those of high tensile steel alloys. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on forming, heat treating, machining, and joining. Filing Code: Al-26. Producer or source: High Duty Alloys Ltd.