REM-CRU C-110M titanium-base alloy was developed for a formable, structural sheet material with improved strength-weight properties in the intermediate temperature range. This alloy was coded as RC-130-A prior to March, 1954. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as creep and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ti-6. Producer or source: Rem-Cru Titanium Inc..