Abstract

CARPENTER No. 5-317 is a nickel-chromium medium carbon steel for high combination of hardness and toughness in heat treated condition. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-27. Producer or source: Carpenter.