Abstract

AMPCO METAL-8 is a wrought alpha phase aluminum bronze possessing high tensile, impact and faigue characteristics. It is non-magnetic and resistant to sparking. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, machining, and joining. Filing Code: Cu-23. Producer or source: Ampco Metal Inc..