ALLEGHENY LUDLUM STAINLESS TYPE 440A is a hardenable high-carbon chromium steel designed to provide stainless properties with high hardness. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-38. Producer or source: Allegheny Ludlum Corporation.