DOWMETAL HK31XA is a magnesium-thorium-zirconium alloy having good high temperature creep resistance, and is recommended for applications at elevated temperatures. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on heat treating, machining, and joining. Filing Code: Mg-20. Producer or source: The Dow Chemical Company.