MEEHANITE GE is a medium strength iron having high damping capacity, self-lubricating properties, and good machinability. It combines the good properties of both cast iron and steel. Applications include machine tools, gears, shafts, housings, pump bodies, valve bodies, steam cylinders, cylinder liners, casings, cylinder heads, and governor frames. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness. It also includes information on casting, heat treating, and machining. Filing Code: CI-12. Producer or source: Meehanite Metal Corporation.