Abstract

WORTHITE is a high nickel-chromium acid-resisting steel for the chemical and process industries. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as casting, forming, heat treating, machining, and joining. Filing Code: SS-24. Producer or source: Worthington Corporation.