Abstract

ARMCO NITRONIC 40 Stainless Steel is one of the most versatile austenitic stainless steels with a room-temperature yield strength about twice that of AISI Types 304, 321 and 347. In addition, NITRONIC 40 has remarkably good elevated temperature properties and oxidation resistance. It retains high toughness down to -423 F. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-327. Producer or source: Armco Advanced Materials Corporation. Originally published as Nitronic 40, May 1976, revised August 1990.