Abstract

ULTEM 6100 and 6200 are glass reinforced and ULTEM 6202 is a mineral filled copolymer resin. For properties of the unreinforced resin, ULTEM 6000, see Alloy Digest P-27, June 1991. These are high temperature materials that are particularly suitable for military electrical components which must survive 200 C testing. This datasheet provides information on physical properties, hardness, tensile properties, and compressive and shear strength as well as fracture toughness. It also includes information on corrosion resistance. Filing Code: Cp-16. Producer or source: G. E. Plastics.