Abstract

DURA-BAR G1A alloyed iron is engineered for the glass mold industry. It is produced by continuous casting which results in fine graphite flake size and size and fine matrix structure. This datasheet provides information on composition, microstructure, and hardness. It also includes information on heat treating and machining. Filing Code: CI-61. Producer or source: Federal Bronze Products Inc..