Abstract

AA 4032 has a comparatively low coefficient of thermal expansion and good forgeability. The alloy takes on an attractive dark gray appearance when anodized which may be desirable in architectural applications. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength as well as fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-305. Producer or source: Various aluminum companies.