Abstract
VERTON OF-700-10 is a long glass fiber reinforced polyphenylene sulfide. It has been engineered to maximize the benefits of long fiber reinforcement while maintaining the ease of processing and good fiber despersion associated with conventional short fiber reinforced compounds. Impregnation of the fibers with the resin is by pultrusion rather than the usual compounding extruder. This enables a high level of impregnation to be achieved without damaging the fibers. This datasheet provides information on tensile properties as well as fracture toughness. It also includes information on casting. Filing Code: Cp-9. Producer or source: ICI Advanced Materials.
This content is only available as a PDF.
Copyright © ASM International® 1996
1996
ASM International
You do not currently have access to this content.