Abstract

Ti-3A1-2.5V is a near-alpha titanium alloy offering 20-50% higher tensile properties than the strongest commercially pure grade of titanium at both room and elevated temperatures. Normally furnished in the annealed, or in the cold-worked stress-relieved condition, Ti-3A1-2.5V titanium alloy features excellent cold formability and good notch tensile properties, as well as corrosion resistance in many environments. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-95. Producer or source: Titanium alloy mills.