Abstract

ASTM A 36 defines the primary or basic structural steel for construction. The specification covers rolled carbon steel for structural purposes. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on machining and joining. Filing Code: CS-126. Producer or source: Bethlehem Steel Corporation.