Abstract

CARPENTER VACUMET HYMU "800" ALLOY is a vacuum melted nickel-iron-molybdenum alloy available in strip form for the manufacture of laminations and tape toroids. This datasheet provides information on composition, physical properties, and hardness. It also includes information on heat treating. Filing Code: Ni-378. Producer or source: Carpenter.