Abstract
ULTEM 2100, 2200, 2300 and 2400 resins have high heat resistance, inherent flame resistance with low smoke evolution, broad chemical resistance and outstanding processability. Glass reinforcment provides increased rigidity and dimensional stability while maintaining good processing features. The ULTEM 2000 series is available in both low viscosity and mold release grades in addition to the standard grades. This datasheet provides information on physical properties, hardness, tensile properties, and compressive and shear strength as well as fracture toughness. Filing Code: Cp-5. Producer or source: G. E. Plastics.