MAGNUM ABS 9408 High Heat Grade is specifically designed for heat resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. Filing Code: P-21. Producer or source: The Dow Chemical Company, Dow Plastics.