Abstract

NICKEL VAC N was originally developed as a container material for molten fluoride salts. It is a moderate strength, solid solution strengthened alloy with good oxidation resistance to 1800 F. It has excellent resistance to fluoride salts in the range 1300-1600 F. It is produced by vacuum induction melting followed electroslag remelting. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-388. Producer or source: Teledyne Allvac.