Abstract

SAE 9310 is a nickel-chromium-molybdenum carburizing steel with excellent toughness in both core and case. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on heat treating and machining. Filing Code: SA-444. Producer or source: Alloy steel mills and foundries.