Abstract

TAXTIX 123 and TACTIX 138 resins cured with TACTIX H31 and TAXTIX H41 hardeners are specifically designed to maximum performance properties most critical to advanced composites. This datasheet provides information on composition, physical properties, tensile properties, and compressive strength. Filing Code: P-15. Producer or source: The Dow Chemical Company, Dow Plastics.