KBI-10 alloy is a high-strength tantalum-tungsten alloy. It has excellent strength at high temperatures. This gives it serviceability as an aerospace material. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ta-12. Producer or source: Cabot Corporation.