Abstract
STAVAX ESR is a hardenable stainless steel designed for plastics molding service. Being stainless, it offers reduced mold maintenance costs and constant cooling efficiency (non-corroding water cooling channels) and enhanced productivity throughout the life of the mold. It is electroslag refined (ESR). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: SS-507. Producer or source: Uddeholm Corporation.
This content is only available as a PDF.
Copyright © ASM International® 1996
1996
ASM International