COPPER No. C15715 is a dispersion hardened copper fabricated by powder metallurgy techniques. Its electrical conductivity is 92% IACS and its annealed tensile strength (0.050 in. diameter wire) is 52000-66000psi, depending on annealing temperature. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-547. Producer or source: SCM Metal Products.