Abstract

Titanium Development Association commercially pure wrought titanium, Grade 4 is used in equipment where resistance to corrosion in chemical, marine and other industries is required. At a guaranteed 80,000 psi minimum mill annealed tensile strength, titanium Grade 4 is the strongest of the commercially pure grades. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-92. Producer or source: Titanium alloy mills.