IncoMAP alloy Al-9052 is a high-strength, corrosion resistant aluminum alloy made by the mechanical alloying process. It is dispersion strengthened by oxides and carbides. Its density is 5% less than age hardenable aluminum alloys of comparable strength. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-296. Producer or source: Inco Alloys International Inc..

This content is only available as a PDF.
You do not currently have access to this content.