Abstract

UNS N05502 provides improved machinability. It maintains high strength up to about 800 F and has good corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: Ni-369. Producer or source: Nickel-base alloy producers.

This content is only available as a PDF.
You do not currently have access to this content.