PYROWEAR Alloy 53 is a carburizing steel with good temper resistance and high case hot hardness combined with high core impact strength and fracture toughness. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on forming and heat treating. Filing Code: SA-443. Producer or source: Carpenter.