Abstract

GRILON PV-15H is a 15% glass-fiber reinforced grade offering intermediate rigidity and strength characteristics. This datasheet provides information on physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on casting. Filing Code: Cp-4. Producer or source: EMS-American Grilon Inc..