Abstract
GALL-TOUGH Stainless is an austenitic stainless steel which possesses superior self-mated galling and metal-to-metal wear resistance. It is stronger and has better high-temperature oxidation resistance than AISI Type 304 stainless. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-510. Producer or source: Carpenter.