Abstract
PYROMET Alloy 80A, a high-temperature nickel-base alloy is characterized by its excellent creep resistance, high fatigue properties under very arduous conditions and high oxidation resistance. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and machining. Filing Code: Ni-189. Producer or source: Carpenter Technology Corporation. Originally published April 1973, revised October 1989.