Abstract

BRIGHTRAY Alloy 35 is an iron-nickel-chromium alloy containing long-life rare-earth additions. It is suitable for applications subject to frequent switching and wide temperature fluctuations to a maximum operating temperature of 1050 C(1920 F). It has a relatively large temperature coefficient of resistance which must be taken into account in design calculations. This datasheet provides information on composition, physical properties, and tensile properties. Filing Code: Fe-85. Producer or source: Inco Alloys International Inc..