Abstract

INCOLOY alloy 825 is a nickel-chromium-iron alloy with additions of molybdenum, copper, and titanium. It is resistant to chloride-ion stress-corrosion cracking, to pitting and crevice attack, and to corrosion in both oxidizing and reducing media. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-109. Producer or source: Inco Alloys International Inc.. Originally published December 1965, revised June 1988.