Abstract
CARPENTER HIPERCO 50 is a magnetic soft alloy used primarily as magnetic core in electrical equipment requiring high permeability at very high magnetic flux densities. These magnetic characteristics permit weight reduction, reduction of copper turns and insulation in the end product in comparison to magnetic alloys having lower permeabilities in the same magnetic field range. This datasheet provides information on composition and physical properties. It also includes information on heat treating and machining. Filing Code: Co-83. Producer or source: Carpenter.