UNS No. Z35840 is a zinc-aluminum-copper alloy that offers exceptionally high strength (58,000 to 64,000 psi tensile strength as cast) at modest cost. It performs best in thin-walled castings (down to 0.10 inch) which means reduced weight and lower material costs when castings are redesigned. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness, creep, and fatigue. It also includes information on corrosion and wear resistance as well as forming, heat treating, machining, and surface treatment. Filing Code: Zn-44. Producer or source: Zinc alloy producers.