Abstract
UNS C16200 is a solution strengthened electrical conducting copper. It is additionally hardenable by cold work. Cadmium confers high anneal resistance to the alloy. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-541. Producer or source: Copper alloy producers. See also Alloy Digest Cu-535, February 1988.