NIMONIC alloy 86 is a nickel-base high-temperature alloy with exceptionally good cyclic oxidation resistance at 1050 C (1922 F). The alloy has good workability, ductility and weldability. It is intended principally for use in sheet form. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-351. Producer or source: Inco Alloys International Inc..