Abstract

Copper Alloy No. C44300 is a copper-zinc-tin alloy inhibited by arsenic; it is commonly known as inhibited admiralty metal or admiralty brass. It has a good combination of strength and ductility and good resistance to general corrosion. The small addition of arsenic (nominally 0.06%) is made to minimize the alloy's susceptibility to dezincification and stress corrosion. It is used widely for condenser, evaporator and heat-exchanger tubes and associated applications. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-526. Producer or source: Copper and copper alloy mills.