BRUSH WELLMAN S-200F is beryllium strengthened by a dispersion of beryllium oxide (1.5%). It has moderate strength and moderate ductility (A minumum of 2.0% elongation). Its uses include optical equipment, nuclear reactors, instrumentation, optical substrates, satellite structures and solar arrays. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Be-4. Producer or source: Brush Wellman Inc..
BRUSH WELLMAN S-200F, chemical composition, corrosion-resistant alloys, ductility, elasticity, fracture toughness, heat treatability, instrumentation, joinability, machinability, nuclear reactors, optical equipment, optical substrates, physical properties, satellite structures, solar arrays, tensile properties, workability
This content is only available as a PDF.
Copyright © ASM International® 1996
1996
ASM International
You do not currently have access to this content.