Abstract
UNS No. A02060 is an aluminum-mold casting alloy that responds to an age-hardening heat treatment. It is recommended for applications that require a combination of high tensile properties and good machinability. Among its many uses are fuel pump bodies, aircraft fittings and seat frames for railway passenger cars. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information on high temperature performance as well as casting, heat treating, machining, and joining. Filing Code: Al-285. Producer or source: Various aluminum companies.
aircraft fittings, cast aluminum alloys, castability, chemical composition, compressive strength, elasticity, fatigue properties, fuel pump bodies, hardness, heat treatability, high-temperature alloys, joinability, machinability, physical properties, seat frames, shear strength, tensile properties, UNS A02960, UNS A02960
This content is only available as a PDF.
Copyright © ASM International® 1996
1996
ASM International
You do not currently have access to this content.