Abstract
ZHC COPPER is a high-electrical-conductivity alloy developed to satisfy the requirements of high-power electronic circuits. It has high strength compared to other metals of equivalent conductivity, good bend formability, excellent stress-relaxation resistance and is readily soldered. It also is known as Olin Alloy C151. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Cu-520. Producer or source: Olin Brass.