Abstract
BRUSH WELLMAN S-65B is a grade of beryllium strengthened by a dispersion of beryllium oxide. It has moderate strength and fairly low ductility (a minimum of 3% elongation). Its uses include optical applications, nuclear reactors, instrumentation, X-ray windows, high-speed computer parts, audio components and aerospace structural applications. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Be-3. Producer or source: Brush Wellman Inc..
aerospace structures applications, BRUSH WELLMAN S-65B, chemical composition, corrosion-resistant alloys, ductility, elasticity, electronic components, fracture toughness, heat treatability, instrumentation applications, joinability, machinability, nuclear reactors, optical applications, physical properties, tensile properties, workability, X-ray windows
This content is only available as a PDF.
Copyright © ASM International® 1996
1996
ASM International
Topics
X-ray detectors
Air and spacecraft
Electrical and electronics
Nuclear reactors
Corrosion-resistant alloys
Beryllium alloys
Chemical composition
Heat treatability
Joinability
Machinability
Workability
Elastic modulus
Fracture toughness
Ductility
Tensile properties
Physical properties
Thermal properties
You do not currently have access to this content.